Causes and Solutions of Induction Furnace Earth Leakage


Reasons for Induction Furnace Earth Leakage



A common accident in an induction furnace block is a leak through the hearth. If an accident occurs, if no measures are taken, it will cause the copper tube of the coil to rupture, and the molten iron and coolant will explode. reason:


1. The quality factor of the materials used in the construction of the furnace: generally, the lining material of quartz acid is used. The silicon content of quartz sand and quartz powder should be more than 99.5%, in the form of oily crystals, transparent and free of impurities. Generally, high-purity quartz sand (silicon content 99.85%, hardness 8, density 2.65, refractoriness 1850 degrees) is used.


2. Binder factors used in furnace construction: traditional furnace construction methods generally use boric acid as a binder. Boric acid has both advantages and disadvantages: the advantage is that it adheres quickly at low temperatures, generally starting at 600-700 degrees; the disadvantage is that it is not resistant to high temperatures and erosion. Under high-temperature conditions, boiling will occur in the lower part of the furnace wall, and the number of furnaces used will be greatly reduced. It is recommended to use boric acid as a binder because boric acid has the characteristics of high-temperature bonding, high melting point, high-temperature resistance, and corrosion resistance.


Induction Furnace Earth Leakage Solution Technical Solution


In order to overcome the shortcomings of high coil maintenance cost and long maintenance cycle of the induction coil, a method to quickly solve the leakage and ignition of the induction coil of the induction heating furnace can eliminate the phenomenon of leakage and ignition of the induction coil in a short period of time. The induction coil can be put into use again in a short time, and at the same time, the overall service life of the induction coil can be greatly improved.


The induction furnace earth leakage solution technical solution is a method for quickly solving the induction coil leakage and ignition of the induction heating furnace, comprising the following steps:


1. First confirm the leakage and ignition parts of the induction coil, and then remove the guide rail on the induction coil;

2. Remove the leakage on the induction coil and the damaged insulating material on the ignition part to expose a section of copper tube wound on the induction coil;

3. Re-insulate the exposed section of copper pipe;

4. Apply a layer of refractory mud on the surface of the newly insulated part of the induction coil;

5. Reinstall the guide rail on the induction coil that has been coated with refractory mud;

6. Use the residual heat of the heated workpiece to dry the newly applied refractory mud.


This induction furnace earth leakage solution technical solution quickly solves the technical solution of the induction coil leakage and ignition method of the induction heating furnace. It does not need to destructively repair the entire induction coil, as long as the leakage and ignition parts are partially repaired, it can be repaired Eliminate the phenomenon of leakage and ignition of the induction coil in a short period of time, so that the induction coil can be put into use again in a short period of time, and at the same time, the overall service life of the induction coil can be greatly improved.


This induction furnace earth leakage solution has the characteristics of simplicity, reasonableness, speed, and practicality. It can be repaired at the user terminal, and it is very practical in the actual production of the enterprise. As long as the induction coil is not completely damaged, the present invention can be used almost method has great economic significance.



评论

此博客中的热门博文

Application Range of Medium Frequency Induction Furnace

  Application Range of Medium Frequency Induction Furnace (1) Intermediate frequency induction furnace is used for forging and rolling 1. Wheel forgings, ring forgings, shaft forgings, cylinder forgings, gear forgings, stainless steel forgings, and large flanges. 2. Hot heading of standard parts and fasteners, such as heating for tempering, forging, and extrusion of high tools. 4. Quenching and tempering of bar materials (2) Intermediate frequency induction furnaces are used for smelting   Including the smelting of steel, gold, silver, copper, and aluminum, especially in the foundry industry (3) Intermediate frequency induction furnace is used for heat treatment 1. Heat treatment of various hardware tools and hand tools. Such as pliers, wrenches, screwdrivers, hammers, axes, etc. 2. High-frequency hardened crank pins, sprockets, camshafts, valves, various rocker arms, rocker shafts for various auto parts and motorcycle parts; various gears, spline shafts, transmission axles, High-f...

Induction Furnace Voltage

Induction Furnace Voltage The induced voltage of the intermediate frequency furnace often exists on the inductor coil, the furnace mouth plate, the water-cooled guide rail, and the furnace body bracket. So, what is the reason for the induction voltage of the induction furnace? Next, we will talk about the induced voltage of the intermediate frequency furnace. When the induction coil of the intermediate frequency furnace is working, when an alternating current passes through the coil, an alternating magnetic field is established in the space around the coil. An induced electromotive force is generated in the metal blank in the alternating magnetic field. We often regard the blank as a closed circuit with only one turn of the coil. When the induced electromotive force is generated, an alternating self-circulating circulating current—eddy current is generated in the circuit. Induction heating is to use the heat energy generated by this eddy current to heat the metal blank. The water-cool...

Troubleshooting of Medium Frequency Furnace

Troubleshooting of Medium Frequency Furnace This article introduces the faults and solutions of medium frequency furnace. 1. Fault phenomenon: large DC current, low DC voltage, and if the voltage, dull equipment sound, over-current protection. Analysis and treatment: the thyristor with one arm of the inverter bridge may be short-circuited or open-circuited, resulting in the operation of the three-arm inverter bridge. Use an oscilloscope to observe the voltage drop waveform of the thyristor on the four bridge arms of the inverter bridge. If the voltage drop waveform of the thyristor on one bridge arm is a line, the thyristor has been through; if it is a sine wave, the thyristor has not been through. Replace the through thyristor; find out the reason why the thyristor is not turned on. 2. Fault phenomenon: when the heavy load cold furnace is started, all electrical parameters and sounds are normal, but the power cannot be raised, and overcurrent protection. Analysis and ...